A buyer in Dubai asked for 300 pairs of gold hoop earrings. She said 18K. We sent a quote. She came back two days later and said her retail customers actually want 22K. We re-quoted. Then she asked why the 22K price was only 12 percent higher than 18K when the gold content was 22 percent higher. The answer is the alloy, the casting yield, and the plating - not just the gold price per gram. Karat choice for export is one of the most misunderstood decisions in wholesale gold jewelry, and it varies sharply by destination market.
The Wikipedia entry on karat explains the ratio: 24K is pure gold, 18K is 75 percent gold, 14K is 58.5 percent, 10K is 41.7 percent. But the export reality is that each destination market expects a different karat, a different color, and a different hallmark. Getting this wrong means your jewelry sits in customs or fails a local assayer test. We have seen shipments held at Jebel Ali for three weeks because the 18K stamp was read as 14K by a local inspector.
01Which karat sells in which market
22K and 21K. Demand is concentrated in the Middle East, South Asia and parts of North Africa. Gold is bought as much for value as for adornment, so higher purity matters. We cast 22K in yellow gold only. The typical 22K piece is a hoop earring, a thin bracelet, or a pendant with minimal setting. 18K. The default for EU, UK, US and East Asian export jewelry. 18K holds prongs and detail better than 22K, and it resists scratching through daily wear. We cast 18K in yellow, rose and white. This is the karat we recommend if you are selling to a mixed-market retailer. 14K. The US and Canadian daily-wear default. Cheaper than 18K, harder, and the karat most US retailers stock. 14K holds a prong better than 18K because it is alloyed with more copper and silver. 10K. Entry-level US market only. Below 10K, US FTC rules do not allow the piece to be called gold without a qualifier.
Our own export mix over the last 12 months: 18K at 52 percent, 14K at 28 percent, 22K at 14 percent, 10K at 6 percent. If you are building a mixed-market assortment, 18K is the safest default. We have also noticed that 14K rose gold is growing fast in the US market, up from 4 percent of our US orders in 2023 to 11 percent in 2025.
02Color, alloy and plating
White gold is never pure gold. It is alloyed with nickel, palladium or silver, then rhodium plated. The nickel alloy version is cheaper but fails EU nickel release limits; we use palladium white gold for EU-bound orders. Rose gold uses copper and a small amount of silver. Yellow gold uses silver and copper in a ratio tuned to the target color. Plating adds 0.2 to 0.5 micron of rhodium on white gold; on yellow and rose gold we do not plate, because plating dulls the color.
For pricing context, see K-gold versus silver moissanite price bands and K-gold setting durability for retail. Gold price is passed through at the daily Shanghai Gold Exchange fix, plus a 12 to 18 percent making charge depending on karat and complexity. The making charge is higher on 22K because the soft alloy needs more hand finishing. We also see a 3 percent higher scrap rate on 22K, because the soft metal marks during polishing and has to be re-finished. That scrap rate is baked into the unit price, which is why 22K is not simply 22 percent more expensive than 18K. Buyers who compare only the gold price per gram usually get a surprise on the invoice.
White gold is never pure gold. It is alloyed with nickel, palladium or silver, then rhodium plated. The nickel alloy version is cheaper but fails EU nickel release limits; we use palladium white gold for EU-bound orders. Rose gold uses copper and a small amount of silver. Yellow gold uses silver and copper in a ratio tuned to the target color. Plating adds 0.2 to 0.5 micron of rhodium on white gold; on yellow and rose gold we do not plate, because plating dulls the color.
03FAQ
Is 18K gold better than 14K?
Not universally. 18K has more gold color and value feel; 14K is harder and more scratch-resistant. For daily-wear rings, 14K lasts longer. For statement earrings, 18K looks richer.
Can I mix karats in one order?
Yes, but each karat requires a separate alloy melt. We combine orders of the same karat across buyers to share the melt cost. Mixed karats on one PO add about 3 days lead time.
Does 22K gold hold moissanite prongs?
Barely. 22K is soft and prongs can bend after 6 to 12 months. We recommend 18K minimum for moissanite settings, and 14K for rings worn daily.
Do you stamp the karat on every piece?
Yes, inside the band or on the pendant bail, plus our maker mark. For EU orders we also supply an assay certificate on request.
04Export your karat order
Tell us the destination country and the karat you need. We will confirm alloy color, hallmark and plating, quote at the daily gold fix, and supply assay paperwork. MOQ is 10 pieces per karat. See lab grown diamond chain factory supply for matching stone work.