K Gold Wholesale: Incoming QC Checklist for Buyers
Factory notes/
Your cartons clear customs on a Tuesday. The courier drops them at 9:04am. By 9:06am somebody in your warehouse has a box cutter in hand and no plan. That gap between delivery and the first signature is where most K gold wholesale disputes are born, and it has nothing to do with luck.

Your cartons clear customs on a Tuesday. The courier drops them at 9:04am. By 9:06am somebody in your warehouse has a box cutter in hand and no plan. That gap between delivery and the first signature is where most K gold wholesale disputes are born, and it has nothing to do with luck.

I have spent twelve years on the receiving side of this trade, first inspecting incoming goods for a US importer, now running QC at a factory in Guangxi. Below is the receiving script I would hand a new hire on day one. Print it, tape it to the inspection bench, and work through it in order.

01Before the Truck Arrives: Minutes 0 to 10

Do not open a single poly bag until three things are on the bench: your purchase order, the factory's pre-shipment inspection report, and a calibrated scale reading to 0.001 g. If the PIs do not include karat, gram weight per piece, stone count, and clasp type, ask for a corrected copy before you cut tape.

Photograph all six sides of each carton, including the seal and the shipping label, while the cartons are still closed. This takes ninety seconds and settles every later argument about crushed corners or water damage.

Tools to stage on the bench

  • 10x loupe and a loupe light, not a phone camera zoom
  • Digital scale rated to 0.001 g and a known 10 g test weight
  • Electronic gold tester or XRF unit, plus test acids as backup
  • Digital calipers for band width and stone diameter
  • Magnet strong enough to lift a paperclip
  • Printed count sheet and a red pen

02Minutes 10 to 25: Carton Count and Identity Match

Count inner boxes against the packing list before you count pieces. A missing inner box is a shipping problem; a short count inside a sealed box is a production problem, and you handle them differently. Write the number you actually see, not the number you expect.

Pull three random SKUs and compare the physical item to the photo on the PO. Karat stamp, stone color grade, and setting style must match. In K gold wholesale, the most common incoming failure is not a bad stone, it is a 10K stamp on a 14K order because two lines ran back to back on the same bench.

Stamp and hallmark check

Read every stamp under the loupe at an angle where the light rakes across the recess. Shallow, hand-scratched stamps on a production order are a red flag for a workshop using a hand punch instead of a laser. Confirm the country-of-origin mark your market requires is present and legible.

Count inner boxes against the packing list before you count pieces. A missing inner box is a shipping problem; a short count inside a sealed box is a production problem, and you handle them differently. Write the number you actually see, not the number you expect.

03Minutes 25 to 55: Weight and Karat Verification

Weigh a 10-piece sample, not one piece. Single-piece weighing hides variance. Record each weight, then compare against the tolerance you agreed in writing. For cast K gold wholesale jewelry, plus or minus 3 percent per piece is a normal commercial band; anything tighter needs to be negotiated before production, not after.

Run the electronic tester on the inside of a band or the back of a pendant, never on a prong tip. Two passes per piece, and if the two readings disagree by more than half a karat, set the piece aside for XRF. Do not clean the item first; residue and polishing compound can skew a surface reading.

CheckSample sizeAccept bandAction if failed
Piece weight10 pcs per SKUWithin 3 percent of specWeigh full SKU
Karat reading100 percent of piecesMatches stampQuarantine, XRF
Stone diameter20 stones per SKUWithin 0.1 mmReject lot
Clasp pull test5 pcs per SKUNo deformation100 percent recheck

04Minutes 55 to 80: Stone and Setting Inspection

Moissanite and lab-grown stones are graded by the same color and clarity language as mined goods, but the failure modes differ. Moissanite shows doubling under the loupe at a tilted angle; lab-grown diamond does not. Know which stone you bought before you judge it.

Check prong height on every third piece. A prong sitting 0.2 mm too high catches on knitwear and comes back as a return six weeks later. Run a fingernail along the gallery; if it snags, the finishing bench rushed the polish.

Certificate cross-check

GRA cards should match the stone measurement and the piece count on the packing list. For orders above a stated value, IGI reports should be present per stone with matching report numbers. Scan the QR or look up the number while the box is open, not next week. A mismatched report number is a documentation error you can still fix cheaply on the day of delivery.

Receiving is the only moment when every party still has the goods, the paperwork, and the leverage in the same room. Spend the time.

05Minutes 80 to 100: Chain, Clasp, and Finish

Hang each chain and let it fall. Kinks, twists, and uneven link spacing show up immediately under gravity and are invisible when the chain is coiled in a bag. Flex every clasp ten times and listen. A crisp click with no grit is what you want.

Check the plating thickness on two-tone pieces at the high-wear point, usually the clasp tongue and the first link. Rhodium over white gold should read even in color with no copper bleed at the edges.

  • Chain length measured flat, not stretched
  • Clasp spring tension tested by hand, ten cycles
  • Earring post solder joint inspected at the base
  • Ring sizing verified with a mandrel on three pieces
  • Surface polish checked under raking light, not overhead light

06Minutes 100 to 120: Paperwork, AQL, and the Sign-Off Decision

Now run your AQL sample. For a typical K gold wholesale shipment, General Inspection Level II with AQL 2.5 for major defects and 4.0 for minor is the commercial norm. Major means the piece cannot be sold: wrong karat, missing stone, broken clasp. Minor means cosmetic: light polish haze, a stamp slightly off center.

Count certificates, count poly bags, count return labels if included. Photograph the full layout of the inspected sample flat on the bench with the PO visible in frame. That single image has resolved more claims than any email thread.

If the shipment passes, sign and release to stock. If it fails on a major defect rate above your AQL line, do not refuse the whole container. Quarantine the failed SKU, release the clean SKUs, and send the defect photos the same day. Partial release keeps your shelves full while the claim runs.

07Why Our Receiving Numbers Look Different

Buyers who move from trading companies to a direct factory usually notice three things change at once: cost lands roughly 20 percent lower, lead time shortens by a similar margin, and first-pass yield on incoming inspection climbs. The reason is structural, not magical. There is no middle layer re-packing goods, so nobody re-inspects and re-bags before you do, and defects get caught at the bench instead of at your dock.

Our line runs a three-stage check: incoming stone verification before casting, in-process inspection at setting and polishing, and a pre-ship AQL pull. Custom orders start at 30 pcs per style, stock items ship from 1 pc, production runs 12 to 18 days, and DDP delivery lands in 5 to 8 days. Payment is T/T with 30 percent deposit, and PayPal works for sample orders. Reach the team at service@holycome.com or WhatsApp +86 133 7744 7107.

08Frequently Asked Questions

What is the minimum order for K gold wholesale?

Stock styles ship from 1 piece, which suits buyers testing a new market or filling a single client request. Custom designs in your own specification start at 30 pcs per style, and that volume is what makes a dedicated casting run worthwhile.

How long does production and delivery take?

Standard production runs 12 to 18 days after deposit and artwork approval. DDP delivery adds 5 to 8 days to your door, so a clean custom order typically lands inside a month from confirmation.

How is pricing calculated, and what certificates come with it?

Price is quoted per piece on karat, gram weight, stone type and size, and setting labor, so a change in stone grade moves the number directly. Moissanite ships with GRA cards, and lab-grown diamond orders above the agreed value include IGI reports per stone.

Send us your next PO or a short list of styles you want to test, and we will come back with a per-piece quote, current stock availability, and a sample you can run through this exact checklist before you commit to volume.

Need a quote on this?Send stone, size and quantity — we reply with costed options inside one working day.
Request pricing →

Written by the Holycome manufacturing & quality team. Every figure and claim in this article comes from our own production floor in Wuzhou, China — in-house casting, stone setting and a three-pass quality inspection we have run since 2008.

Materials are tested for nickel, lead and cadmium release by SGS and CTT International; moissanite centre stones ship with their GRA warranty card and report. We also hold an independent SMETA / Sedex ethical-trade audit and a Hong Kong Customs AML registration.

Reviewed for accuracy by our quality team before publication. Last updated .

cta-row" style="margin-top:40px;"> Inquiry Custom Jewelry